欧美大片高清,一本久久综合亚洲鲁鲁,不卡的av影片,台湾佬中文娱乐网欧美电影

What is the cause of yellowing during CPVC injection molding
欄目:Industry News 發布時間:2021-06-03 15:19
Recently, the customer service received a new development of CPVC injection molding customer for help. The customer said that when we purchased our CPVC injection plastic, we found that the product was easy to turn yellow and the processing...
Recently, the customer service received a new development of CPVC injection molding customer for help. The customer said that when we purchased our CPVC injection plastic, we found that the product was easy to turn yellow and the processing was difficult. We asked for assistance. Our customer service staff first checked our workbook according to our CPVC injection molding process, and checked the processing temperature, speed and pressure with the customer. The customer indicated that they were all in accordance with the processing instructions. So the customer service will feedback this problem to the technical engineer for the first time, and ask the engineer to immediately call the customer to solve the problem.

After the technical and customer service docking has completed this information, it has been docked with the customer. After in-depth communication, we understand that the equipment used by customers has been PVC injection molding products, but it is not a special equipment for PVC injection molding. Previously produced PVC injection molding products, the structure is relatively simple, so the molding problems are not big. However, due to the relatively complicated mold structure of CPVC, the fluidity of CPVC injection molding is relatively poor compared with PVC injection molding. The shear heat in the CPVC injection molding process is too high, causing slight decomposition of the CPVC material to cause yellowing.

According to the current status of the customer's equipment, Jiahong Plastics Engineer recommends that the length of the nozzle be shortened and the flow path be modified or enlarged to avoid the material pressure being decomposed due to the instantaneous pressure increase of the injection glue, which can make the material smooth. The injection into the mold to solve the problem of yellowing of CPVC injection products.

Later customer service followed up with the customer, the customer said that according to the recommendations of our engineers to improve the product, has been injection molding, and delivered samples to their end customers to confirm. Yellowing during CPVC injection molding is a problem we noticed when we first developed materials, so engineers can quickly provide solutions when communicating with customers.

Wuxi Jiahong Plastic Technology Co., Ltd. has nearly 30 years of experience in research and development and granulation of modified PVC pellets. The professional technical service team can provide one-stop system solutions for customers. For more information about the product, please visit our official website: www.gzfastfast.com, consult online customer service or call the hotline. Fixed line: 0510-68755207 Mobile: 15190220696, we will be happy to help you.

(Disclaimer: All the tutorials and resources included in this site are from the Internet, and the copyrights are owned by the original author and its website. Although this site strives to preserve the original copyright information, it may not be possible for certain reasons. For the true source, please forgive the original author! If you have any objection to the attribution of the tutorial and resources on this site, please notify Xiaobian immediately, the situation is true, we will delete it as soon as possible.)
主站蜘蛛池模板: 富宁县| 大厂| 宾阳县| 岗巴县| 耿马| 武胜县| 公安县| 皋兰县| 上栗县| 江达县| 阿荣旗| 无为县| 鹤壁市| 黄浦区| 桐庐县| 台安县| 磐安县| 凉山| 曲麻莱县| 白沙| 巴中市| 邮箱| 涞源县| 石狮市| 休宁县| 东乡县| 建阳市| 宜宾县| 阜康市| 灵丘县| 南漳县| 东方市| 吴旗县| 合水县| 哈巴河县| 通州市| 鄂托克旗| 元谋县| 繁昌县| 天祝| 东港市|